Concrete Surface Preparation Guidelines

Proper surface preparation includes the following:

What are CSP Ratings?
For proper bonding of overlays and coatings, it is important that a concrete surface have the correct Concrete Surface Profile or CSP. A CSP rating is a standardized rating that allows you to visually determine the concrete surface roughness

CSP Rating 2

CSP Rating 2

CSP Rating 2

This rating can be achieved with our tooling that carries a 70–80 Grit rating.
For coating applications from 2–3 mil thickness, the surface profile should be a CSP 2.

CSP Rating 3

CSP Rating 3

CSP Rating 3

This rating can be achieved with our tooling that carries a 50 Grit rating.
For coating applications from 4–5 mil thickness, the surface profile should be a CSP 3.

CSP Rating 4

CSP Rating 4

CSP Rating 4

This rating can be achieved with our tooling that carries a 30–40 Grit rating.
For coating applications from 15–50 mil thickness, the surface should be a CSP 4.

CSP Rating 5

CSP Rating 5

CSP Rating 5

This rating can be achieved with our tooling that carries a 25 Grit rating.
For coating applications from 40 mil thickness, the surface should be a CSP 5.